CP Fast Demoulding System Blend Polyols no ka Refrigrtator Insulation-DonCool 103

ʻO ka wehewehe pōkole:

Hoʻohana ʻo Doncool 103 i nā polyols e hoʻohana i ka CP a i ʻole CP/IP ma ke ʻano he mea puhi, e pili ana i nā pahu hau, freezers, a me nā huahana insulation ʻē aʻe.ʻO nā hiʻohiʻona o nā huahana penei

1. ʻO ka hiki ke kahe maikaʻi, ua māhele maikaʻi ʻia ka mānoanoa o ka pua, a haʻahaʻa ka conductivity thermal.

2. Maikaʻi haʻahaʻa haʻahaʻa-mehana dimensional paʻa a me ka maikaʻi cohesiveness.

3. ʻO ka manawa demould he 6-8 mau minuke.


Huahana Huahana

Na Waiwai Kino

Ka nana aku

ʻeleʻele ʻeleʻele ʻeleʻele ʻeleʻele wai

Waiwai hydroxyl mgKOH/g

360-420

ʻO ka viscosity ikaika(25 ℃)  mPa.s

3000-4000

Kaumaha(20 ℃) g/ml

1.06-1.08

Ka Mahana Waihona

10-25

Paʻa Paʻa Mahina 6

Paipai ʻia lākiō

  Pbw
ʻO DonCool 103 hui pū i nā polyols
CP a i ʻole CP/IP
Isocyanate
100
12-14
130-142

ʻenehana a me ka hana hou

ʻenehana a me Reactivity (ʻokoʻa ka waiwai pololei ma muli o nā kūlana hana)

  Ka hui lima lima Mechanical Foaming
Ka Mahana Makana ℃ 20-25 20-25
Ka Mahana Mold ℃ 35-40 35-40
CT s 12-16 8-12
12GT s 75-85 50-70
TFT s 100-120 70-100
Kūʻai kūʻokoʻa kg/m3 25-26 24-25

Nā hana ʻōhū

ʻO ka mānoanoa o ka huʻa ma ka hoʻoheheʻe ʻana GB/T 6343 ≥35kg/m3
Paʻa-paʻa kelepona GB/T 10799 ≥90%
ʻO ka wela wela (15 ℃) GB/T 3399 ≤22mW/(mK)
Ka ikaika hoʻoemi
(perpendicular i ke ala e piʻi ai) GB/T 8813 ≥150kPa
Paʻa paʻa 24h -20 ℃ GB/T 8811 ≤0.5%
  24h 100 ℃   ≤1.0%